Skip to product grid
-
TopHardness82-84 HDTensile Strength35-45 MPaElongation at Break35-40%Izod Impact Strength212 J/m -
Nozzle≥0.4 mmDry before PrintingRequiredPrinting Temp.195-230 ℃Hotbed Temp.50-60 ℃ -
Fully-Enclosed PrintingRecommendedNozzle≥0.4mmPrinting Temp.240-280 ℃Hotbed Temp.80-100 ℃ -
NewViscosity400-500 mPa.s(25℃)Hardness36-46 HDTensile Strength35-45 MPaElongation at Break133%